Characteristics of Triple Nylon Leak
1. General physical property
Test item |
Unit |
Test method |
Measurement value |
|
Tensile strength at break |
Vertical |
kg/cm2 |
JIS-Z-1702 |
400 |
Horizontal |
380 |
|||
Elongation at break |
Vertical |
% |
JIS-Z-1702 |
370 |
Horizontal |
380 |
|||
Tearing strength at right angle |
Vertical |
kg/cm |
JIS-K-6781 |
120 |
Horizontal |
130 |
|||
Impact strength |
kg.cm |
JIS-P-8134 |
11.6 |
|
Piercing strength |
g |
JAS method |
500 |
|
Haze |
% |
JIS-K-6714 |
21.9 |
|
Oxygen permeability |
c.c./m2.day.atm |
ASTM D-1434 |
42.3 |
|
Moisture permeability |
g/m2.day |
JIS-Z-1702 |
17.2 |
|
Heat seal strength |
kg/15 mm |
JIS-Z-1707 |
2.1 |
The above values are examples of measured values for the film thickness of 0.07 mm and not guaranteed values.
2. Electric performance
Test method |
||
(1) Surface resistively(omega sym.) |
JIS-K-6911 |
Surface 1013 |
Inner surface 1013 - 1010 |
||
(2) Half-valued period |
JIS L 1094 |
Inner surface 0.4 |
The above values are examples of measured values and not guaranteed values.
3. Attenuation characteristic
*Attenuation characteristic means the rapidity of escaping electrified electric charge and half life means the time 50% is attenuated.
Triple Nylon Leak Standards
Layflat width: 100 mm to 300 mm |
Thickness: 0.07 mm to 0.1 mm |